EFOX BPIC S75

EFOX BPIC S75 can be used for the polymerization and copolymerization of styrene in the temperature range 95-125°C. The temperature is gradually increased during polymerization. EFOX BPIC S75 can be used as initiator for the solution copolymerization of acrylates and methacrylates in the temperature range 100-170°C, inter alia for coating production. EFOX BPIC S75 can also be applied as an initiator for bulk and suspension copolymerization of acrylates and methacrylates.

EFOX BPIC S75
Chemical Name
Tert-Bütil Peroksi İzopropil Karbonat 75%
Yoğunluk (@20°C) Viskozite (@20°C) Görünüm Renk
0,900 ± 0,005 gr/cm3 2,3 mPa.s Sıvı Renksiz
Aktif Oksijen İçeriği Peroksit İçeriği (BPIC%) Hidroperoksit (TBHP) Toplam Klor İçeriği
6,72 - 6,90 % 74,0 - 76,0 % Max. 0,10 % Max. 150 ppm
SADT CAS No EINECS/ELINCS No UN No
70°C 2372-21-6 219-143-7 3103
PROPERTIES

EFOX BPIC S75 can be used for the polymerization and copolymerization of styrene in the temperature range 95-125°C. The temperature is gradually increased during polymerization. EFOX BPIC S75 can be used as initiator for the solution copolymerization of acrylates and methacrylates in the temperature range 100-170°C, inter alia for coating production. EFOX BPIC S75 can also be applied as an initiator for bulk and suspension copolymerization of acrylates and methacrylates.