EFOX BPIC S75
EFOX BPIC S75 can be used for the polymerization and copolymerization of styrene in the temperature range 95-125°C. The temperature is gradually increased during polymerization. EFOX BPIC S75 can be used as initiator for the solution copolymerization of acrylates and methacrylates in the temperature range 100-170°C, inter alia for coating production. EFOX BPIC S75 can also be applied as an initiator for bulk and suspension copolymerization of acrylates and methacrylates.
Chemical Name | |||
Tert-Bütil Peroksi İzopropil Karbonat 75% | |||
Yoğunluk (@20°C) | Viskozite (@20°C) | Görünüm | Renk |
0,900 ± 0,005 gr/cm3 | 2,3 mPa.s | Sıvı | Renksiz |
Aktif Oksijen İçeriği | Peroksit İçeriği (BPIC%) | Hidroperoksit (TBHP) | Toplam Klor İçeriği |
6,72 - 6,90 % | 74,0 - 76,0 % | Max. 0,10 % | Max. 150 ppm |
SADT | CAS No | EINECS/ELINCS No | UN No |
70°C | 2372-21-6 | 219-143-7 | 3103 |
PROPERTIES | |||
EFOX BPIC S75 can be used for the polymerization and copolymerization of styrene in the temperature range 95-125°C. The temperature is gradually increased during polymerization. EFOX BPIC S75 can be used as initiator for the solution copolymerization of acrylates and methacrylates in the temperature range 100-170°C, inter alia for coating production. EFOX BPIC S75 can also be applied as an initiator for bulk and suspension copolymerization of acrylates and methacrylates. |